UNS C14700 | |
Category | Copper Alloy |
Class | Wrought |
Type | Sulfur bearing copper alloy |
Designations | United States: UNS C14700 |
Composition | |
Element
|
Weight %
|
Cu
|
99.6
|
S
|
0.40
|
Mechanical Properties | |
Properties |
Conditions
|
||
T (°C) |
Treatment
|
||
Density (×1000 kg/m3) | 8.8-8.94 |
25
|
|
Poisson's Ratio | 0.34 |
25
|
|
Elastic Modulus (GPa) | 117 |
25
|
|
Tensile Strength (Mpa) | 221-393 |
25
|
(rod, wire)
|
Yield Strength (Mpa) | 69-379 | ||
Elongation (%) | 52 | ||
Reduction in Area (%) | |||
Note: Elongation is measured in 8 inches. |